מפרט טכני:
נייר התאמת תבניות
מיוחד להתאמות בין שני חצאי תבניות הזרקה
תכונות:
- עובי 0.1 מ"מ
- ניתן להשתמש בתנאי לחות
- טווח עבודה בלחץ 200 - 6000 PSI
- טמפרטורת עבודה מקסימלית 93+ מעלות
Parting Line aligned and Uniform:
• One way to ensure proper mating of the tool halves at the parting line is simply by having a level molding machine and parallel platens.
• Leveling a machine requires three machinist levels.
• If you have shorts and flash, you could have a mold or clamping alignment problem.
• This may not be the case if you are running a high-speed, thin-wall product—the problem may be simply not enough clamp force.
• To help establish whether flash stems from a mold or clamp alignment issue, check parting-line mating.
• In one typical check for uniform clamp pressure at the parting line, blueing agent applied to one mold half will transfer to the other if there is contact at the parting line, but it will not distinguish between low or high touch force.
• More detailed information can be obtained with Mold-Align® paper, which changes color relative to the amount of contact force.